Seco · chipbreaker for negative inserts

M1 chipbreaker

Light roughing and semi-finishing of superalloys and titanium.

One source: Seco Tools, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO S.chipcutting edgebreaker grooveclearance 0°ISO groupS
The edge in section; its ISO groups. Not to scale.

What Seco prints

Insert
Negative
Made for
ISO S (superalloys and titanium)
Cutting area
light cuts, medium
Feed
0.2–0.4 mm/rev (.0079–.0157 in/rev)
Depth of cut
1.5–5 mm (.059–.197 in)
Edge
Positive rake, slightly honed (sharp .GG available)

Source: Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

M1 equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalMSISO S; medium0.13–0.36 mm/revMedium machining, sharp edge, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalPISO S; medium0.15–0.51 mm/revMedium machining of steel, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalUPISO S; medium0.2–0.64 mm/revMedium machining of stainless and high-temperature alloys.

One source: Kennametal, its own catalog

MitsubishiLSISO S; light cutsnot printedFirst recommendation for light cutting of difficult-to-cut materials; alternative for stainless; chip control at depths under the corner radius.

One source: Mitsubishi Materials, its own catalog

MitsubishiMJISO S; light cutsnot printedAlternative for light cutting of heat resistant and titanium alloys; notch-wear resistant for light to medium cuts.

One source: Mitsubishi Materials, its own catalog

MitsubishiMSISO S; mediumnot printedFirst recommendation for medium cutting of difficult-to-cut materials; alternative for stainless.

One source: Mitsubishi Materials, its own catalog

Why M1 for heat-resistant superalloys (Inconel 718)

M1 for heat-resistant superalloys (Inconel 718): Seco’s light cuts and medium geometry for ISO S.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Seco makes M1 (negative) for S in light cuts, medium at 0.2–0.4 mm/rev (.0079–.0157 in/rev); edge: Positive rake, slightly honed (sharp .GG available). Light roughing and semi-finishing of superalloys and titanium.

    One source: Seco Tools, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists M1 for ISO S, medium. Seco Tools’ own catalog is the authority for its geometry.

It agrees with Seco Tools’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)