Kennametal · chipbreaker for negative inserts

UP chipbreaker

Medium machining of stainless and high-temperature alloys.

One source: Kennametal, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO M and S.chipcutting edgebreaker grooveclearance 0°ISO groupMS
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Insert
Negative
Made for
ISO M (stainless steel), S (superalloys and titanium)
Cutting area
medium
Feed
0.2–0.64 mm/rev (.0079–.0252 in/rev)
Depth of cut
1.02–6.35 mm (.04–.25 in)

Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

UP equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiESISO M; mediumnot printedRight- or left-hand alternative for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiGMISO M; mediumnot printedAlternative to LM and MM for stainless; notch-wear resistant for light to medium cuts.

One source: Mitsubishi Materials, its own catalog

MitsubishiMMISO M; medium0.15–0.46 mm/revFirst recommendation for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiMSISO S; mediumnot printedFirst recommendation for medium cutting of difficult-to-cut materials; alternative for stainless.

One source: Mitsubishi Materials, its own catalog

SandvikMMISO M; mediumnot printedFirst choice for medium machining of stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

SecoM1ISO S; medium0.2–0.4 mm/revLight roughing and semi-finishing of superalloys and titanium.

One source: Seco Tools, its own catalog

SecoM5ISO M; medium0.3–0.7 mm/revRoughing with double-sided inserts at high feed in steel, stainless and cast iron.

One source: Seco Tools, its own catalog

SecoMF4ISO M; medium0.15–0.5 mm/revMedium and finishing cuts in stainless.

One source: Seco Tools, its own catalog

SecoMF5ISO M; medium0.2–0.8 mm/revMedium finishing of steel and stainless at high feeds.

One source: Seco Tools, its own catalog

SecoMR3ISO M, S; medium0.2–0.6 mm/revMedium-rough and rough machining of superalloys, titanium, stainless and hardened steel.

One source: Seco Tools, its own catalog

Show 1 more equivalents
More of other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
SecoMR4ISO S; medium0.15–0.5 mm/revDifficult superalloy and titanium work: intermittent cuts and raw surfaces.

One source: Seco Tools, its own catalog

Why UP for austenitic stainless (304, 316)

UP for austenitic stainless (304, 316): Kennametal’s medium geometry for ISO M.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal makes UP (negative) for M, S in medium at 0.2–0.64 mm/rev (.0079–.0252 in/rev). Medium machining of stainless and high-temperature alloys.

    One source: Kennametal, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists UP for ISO M, S, medium, heavy roughing. Kennametal’s own catalog is the authority for its geometry.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)