Kennametal · chipbreaker for negative inserts
MS chipbreaker
Medium machining, sharp edge, stainless and high-temperature alloys.
One source: Kennametal, its own catalog
What Kennametal prints
- Insert
- Negative
- Made for
- ISO M (stainless steel), S (superalloys and titanium)
- Cutting area
- medium
- Feed
- 0.13–0.36 mm/rev (.0051–.0142 in/rev)
- Depth of cut
- 0.76–5.08 mm (.03–.20 in)
- Edge
- Sharp
Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
MS equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Mitsubishi | ES | ISO M; medium | not printed | Right- or left-hand alternative for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | GM | ISO M; medium | not printed | Alternative to LM and MM for stainless; notch-wear resistant for light to medium cuts. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MM | ISO M; medium | 0.15–0.46 mm/rev | First recommendation for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MS | ISO S; medium | not printed | First recommendation for medium cutting of difficult-to-cut materials; alternative for stainless. | One source: Mitsubishi Materials, its own catalog |
| Sandvik | MM | ISO M; medium | not printed | First choice for medium machining of stainless (T-Max P). | One source: Sandvik Coromant, its own catalog |
| Seco | M1 | ISO S; medium | 0.2–0.4 mm/rev | Light roughing and semi-finishing of superalloys and titanium. | One source: Seco Tools, its own catalog |
| Seco | M5 | ISO M; medium | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | MF4 | ISO M; medium | 0.15–0.5 mm/rev | Medium and finishing cuts in stainless. | One source: Seco Tools, its own catalog |
| Seco | MF5 | ISO M; medium | 0.2–0.8 mm/rev | Medium finishing of steel and stainless at high feeds. | One source: Seco Tools, its own catalog |
| Seco | MR3 | ISO M, S; medium | 0.2–0.6 mm/rev | Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel. | One source: Seco Tools, its own catalog |
Show 1 more equivalents
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Seco | MR4 | ISO S; medium | 0.15–0.5 mm/rev | Difficult superalloy and titanium work: intermittent cuts and raw surfaces. | One source: Seco Tools, its own catalog |
Why MS for austenitic stainless (304, 316)
MS for austenitic stainless (304, 316): Kennametal’s medium geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Kennametal makes MS (negative) for M, S in medium at 0.13–0.36 mm/rev (.0051–.0142 in/rev); edge: Sharp. Medium machining, sharp edge, stainless and high-temperature alloys.
One source: Kennametal, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MS for ISO S, light cuts. Kennametal’s own catalog is the authority for its geometry.
- The cross-reference lists it for light cuts; Kennametal gives medium.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)