Chipbreakers · Seco

Seco chipbreaker chart

8 Seco turning chipbreakers, each as Seco’s own catalog prints it, from MF1 for finishing to M5 for heavy roughing. The table gives each one’s ISO groups, cutting area and feed window; each page lists the other makers’ chipbreakers for the same job.

One source: Seco Tools, its own catalog

The six ISO groups, with how many of the maker’s listed chipbreakers are made for each: P 3, M 6, K 1, N none, S 4, H 1.PMKNSH361041
Seco’s listed chipbreakers by ISO group.

Seco turning chipbreakers, lightest cut first

Seco chipbreakers: insert, ISO groups, cutting area and feed window
ChipbreakerInsertISOCutting areaFeed
MF1negativeM, Sfinishing, light cuts0.08–0.3 mm/rev (.0031–.0118 in/rev)
MF4negativeMfinishing, medium0.15–0.5 mm/rev (.0059–.0197 in/rev)
MF5negativeP, Mfinishing, light cuts, medium0.2–0.8 mm/rev (.0079–.0315 in/rev)
M1negativeSlight cuts, medium0.2–0.4 mm/rev (.0079–.0157 in/rev)
MR3negativeM, S, Hmedium, roughing0.2–0.6 mm/rev (.0079–.0236 in/rev)
MR4negativeSmedium, roughing0.15–0.5 mm/rev (.0059–.0197 in/rev)
M5negativeP, M, Kmedium, roughing, heavy roughing0.3–0.7 mm/rev (.0118–.0276 in/rev)
RR6negativeP, Mroughing, heavy roughing0.3–1 mm/rev (.0118–.0394 in/rev)
Sources1