Kennametal · chipbreaker for negative inserts
P chipbreaker
Medium machining of steel, stainless and high-temperature alloys.
One source: Kennametal, its own catalog
What Kennametal prints
- Insert
- Negative
- Made for
- ISO P (steel), M (stainless steel), S (superalloys and titanium)
- Cutting area
- medium
- Feed
- 0.15–0.51 mm/rev (.0059–.0201 in/rev)
- Depth of cut
- 0.76–5.08 mm (.03–.20 in)
Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
P equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Mitsubishi | ES | ISO M; medium | not printed | Right- or left-hand alternative for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | GM | ISO M; medium | not printed | Alternative to LM and MM for stainless; notch-wear resistant for light to medium cuts. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MM | ISO M; medium | 0.15–0.46 mm/rev | First recommendation for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MP | ISO P; medium | 0.15–0.51 mm/rev | First recommendation for medium cutting of carbon and alloy steel; also light cutting, copying and back turning. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MS | ISO S; medium | not printed | First recommendation for medium cutting of difficult-to-cut materials; alternative for stainless. | One source: Mitsubishi Materials, its own catalog |
| Sandvik | MM | ISO M; medium | not printed | First choice for medium machining of stainless (T-Max P). | One source: Sandvik Coromant, its own catalog |
| Seco | M1 | ISO S; medium | 0.2–0.4 mm/rev | Light roughing and semi-finishing of superalloys and titanium. | One source: Seco Tools, its own catalog |
| Seco | M5 | ISO P, M; medium | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | MF4 | ISO M; medium | 0.15–0.5 mm/rev | Medium and finishing cuts in stainless. | One source: Seco Tools, its own catalog |
| Seco | MF5 | ISO P, M; medium | 0.2–0.8 mm/rev | Medium finishing of steel and stainless at high feeds. | One source: Seco Tools, its own catalog |
Show 2 more equivalents
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Seco | MR3 | ISO M, S; medium | 0.2–0.6 mm/rev | Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel. | One source: Seco Tools, its own catalog |
| Seco | MR4 | ISO S; medium | 0.15–0.5 mm/rev | Difficult superalloy and titanium work: intermittent cuts and raw surfaces. | One source: Seco Tools, its own catalog |
Why P for steel
P for steel: Kennametal’s medium geometry for ISO P.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal makes P (negative) for P, M, S in medium at 0.15–0.51 mm/rev (.0059–.0201 in/rev). Medium machining of steel, stainless and high-temperature alloys.
One source: Kennametal, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists P for ISO P, S, medium. Kennametal’s own catalog is the authority for its geometry.
It agrees with Kennametal’s catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)