ISCAR · PVD-coated carbide

IC354 insert grade

IC354 is ISCAR’s PVD-coated carbide grade (PVD, TiCN) for ISO P20–P40 and M10–M30, as ISCAR’s catalog prints it. General use on carbon, alloy and stainless steel at moderate speed and feed.

One source: ISCAR, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P and M.cutting edgecoating PVDsubstrate carbideISO groupPM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
PVD-coated carbide
Coating
PVD, TiCN
Substrate
Tough
ISO P
P20–P40 · steel
ISO M
M10–M30 · stainless steel
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC354

IC354 equivalents by material

Steel · P

Read at P30, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P30
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNP20–P30

One source: Kennametal, its own catalog

MitsubishiVP15TFPVD-coated carbidePVDP20–P40 (core P30)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why IC354 for steel

IC354 for steel: rated P20–P40 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC354 (PVD-coated carbide) for P20–P40: General use on carbon, alloy and stainless steel at moderate speed and feed.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. ISCAR — eCatalog grade data: IC354

Stainless · M

Read at M20, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M20
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNM10–M20

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDM10–M30 (core M20)

One source: Mitsubishi Materials, its own catalog

SandvikGC1115PVD-coated carbidePVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

SecoCP500PVD-coated carbidePVD, (Ti,Al)N + TiNabout M10–M30

One source: Seco Tools, its own catalog

Why IC354 for austenitic stainless (304, 316)

IC354 for austenitic stainless (304, 316): rated M10–M30 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC354 (PVD-coated carbide) for M10–M30: General use on carbon, alloy and stainless steel at moderate speed and feed.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC354

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC354 at P30, M10, M20. ISCAR’s own catalog is the authority for its grade.

It agrees with ISCAR’s catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)