Mitsubishi · PVD-coated carbide
VP15TF insert grade
VP15TF is Mitsubishi’s PVD-coated carbide grade (PVD) for ISO P20–P40, M20–M40 and K20–K40, as Mitsubishi’s catalog prints it. Tough PVD grade for steel, stainless and cast iron, including interrupted cuts.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- PVD-coated carbide
- Coating
- PVD
- ISO P
- P20–P40 (core P30) · steel
- ISO M
- M20–M40 (core M30) · stainless steel
- ISO K
- K20–K40 (core K30) · cast iron
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
VP15TF equivalents by material
Steel · P
Read at P30, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC300 | PVD-coated carbide | PVD, TiCN | P20–P40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | P20–P30 | One source: Kennametal, its own catalog |
| Sandvik | GC4325 | CVD-coated carbide | CVD | P10–P40 (core P25) | One source: Sandvik Coromant, its own catalog |
Why VP15TF for steel
VP15TF for steel: rated P20–P40 (core P30) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates VP15TF (PVD-coated carbide) for P20–P40 (core P30): Tough PVD grade for steel, stainless and cast iron, including interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
Stainless · M
Read at M30, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1028 | PVD-coated carbide | PVD, TiAlN + TiN | M20–M40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | M20–M30 | One source: Kennametal, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | M10–M30 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why VP15TF for austenitic stainless (304, 316)
VP15TF for austenitic stainless (304, 316): rated M20–M40 (core M30) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Mitsubishi rates VP15TF (PVD-coated carbide) for M20–M40 (core M30): Tough PVD grade for steel, stainless and cast iron, including interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Cast iron · K
Read at K30, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | K20–K40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | K20–K30 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why VP15TF for gray cast iron
VP15TF for gray cast iron: rated K20–K40 (core K30) by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates VP15TF (PVD-coated carbide) for K20–K40 (core K30): Tough PVD grade for steel, stainless and cast iron, including interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists VP15TF at P20, P30, M20, M30, K20, K30, S10, S20, S30, H10, H20. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)