Mitsubishi · cermet
MP3025 insert grade
MP3025 is Mitsubishi’s cermet grade (PVD, Ti compound) for ISO P15–P35, as Mitsubishi’s catalog prints it. Coated cermet for steel, interrupted cutting; uniform flank wear for small parts.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- cermet
- Coating
- PVD, Ti compound
- ISO P
- P15–P35 (core P20) · steel
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names MP3025 its first choice for carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), general conditions: finishing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMP3025 equivalents by material
ISO P (steel)
Read at P20, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC30N | cermet | Uncoated | P10–P30 | One source: ISCAR, its own catalog |
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P20–P25 | One source: Kennametal, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why MP3025 for steel
MP3025 for steel: rated P15–P35 (core P20) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates MP3025 (cermet) for P15–P35 (core P20): Coated cermet for steel, interrupted cutting; uniform flank wear for small parts.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists MP3025 at P30. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)