Seco · PVD-coated carbide

CP600 insert grade

CP600 is Seco’s PVD-coated carbide grade (PVD, (Ti,Al)N + TiN) for ISO M20–M40, as Seco’s catalog prints it. Stainless steel and steel wherever edge toughness matters, such as difficult interrupted cuts.

One source: Seco Tools, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO M.cutting edgecoating PVDsubstrate carbideISO groupM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Seco prints

Type
PVD-coated carbide
Coating
PVD, (Ti,Al)N + TiN
Substrate
Very tough micrograin
ISO M
about M20–M40 · stainless steel
Secondary
ISO P, S (Seco names them in its text only)
Operations
turning

Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.

Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

CP600 equivalents by material

ISO M (stainless steel)

Read at M30, the centre of Seco’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M30
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC1028PVD-coated carbidePVD, TiAlN + TiNM20–M40

One source: ISCAR, its own catalog

KennametalKC5025PVD-coated carbidePVD, AlTiNM20–M30

One source: Kennametal, its own catalog

MitsubishiVP15TFPVD-coated carbidePVDM20–M40 (core M30)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDM10–M30 (core M25)

One source: Sandvik Coromant, its own catalog

Why CP600 for austenitic stainless (304, 316)

CP600 for austenitic stainless (304, 316): rated about M20–M40 by Seco.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Seco rates CP600 (PVD-coated carbide) for about M20–M40: Stainless steel and steel wherever edge toughness matters, such as difficult interrupted cuts.

    One source: Seco Tools, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists CP600 at P40, M30, S30. Seco Tools’ own catalog is the authority for its grade.

It agrees with Seco Tools’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)