ISCAR · PVD-coated carbide
IC1028 insert grade
IC1028 is ISCAR’s PVD-coated carbide grade (PVD, TiAlN + TiN) for ISO P20–P50 and M20–M40, as ISCAR’s catalog prints it. Roughing at low speed and high feed, interrupted cuts.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, TiAlN + TiN
- ISO P
- P20–P50 · steel
- ISO M
- M20–M40 · stainless steel
- Operations
- turning, milling
IC1028 equivalents by material
Steel · P
Read at P35, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | P20–P40 (core P30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why IC1028 for steel
IC1028 for steel: rated P20–P50 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC1028 (PVD-coated carbide) for P20–P50: Roughing at low speed and high feed, interrupted cuts.
One source: ISCAR, the maker of the grade , sources [3]
Stainless · M
Read at M30, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | M20–M30 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | M10–M30 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why IC1028 for austenitic stainless (304, 316)
IC1028 for austenitic stainless (304, 316): rated M20–M40 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC1028 (PVD-coated carbide) for M20–M40: Roughing at low speed and high feed, interrupted cuts.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC1028
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC1028 at P20, P30, P40, M20, M30, M40. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)