Sandvik · chipbreaker for negative inserts
MM chipbreaker
First choice for medium machining of stainless (T-Max P).
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Insert
- Negative
- Made for
- ISO M (stainless steel)
- Cutting area
- medium
Source: Sandvik Coromant — Turning Handbook C-1020-18: geometry and grade, first choice for T-Max P and CoroTurn 107 (p. 2) (archived Nov 16, 2026)
MM equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | MS | ISO M; medium | 0.13–0.36 mm/rev | Medium machining, sharp edge, stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | P | ISO M; medium | 0.15–0.51 mm/rev | Medium machining of steel, stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | UP | ISO M; medium | 0.2–0.64 mm/rev | Medium machining of stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Mitsubishi | ES | ISO M; medium | not printed | Right- or left-hand alternative for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | GM | ISO M; medium | not printed | Alternative to LM and MM for stainless; notch-wear resistant for light to medium cuts. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MM | ISO M; medium | 0.15–0.46 mm/rev | First recommendation for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Seco | M5 | ISO M; medium | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | MF4 | ISO M; medium | 0.15–0.5 mm/rev | Medium and finishing cuts in stainless. | One source: Seco Tools, its own catalog |
| Seco | MF5 | ISO M; medium | 0.2–0.8 mm/rev | Medium finishing of steel and stainless at high feeds. | One source: Seco Tools, its own catalog |
| Seco | MR3 | ISO M; medium | 0.2–0.6 mm/rev | Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel. | One source: Seco Tools, its own catalog |
Why MM for austenitic stainless (304, 316)
MM for austenitic stainless (304, 316): Sandvik’s medium geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Sandvik makes MM (negative) for M in medium. First choice for medium machining of stainless (T-Max P).
One source: Sandvik Coromant, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Turning Handbook C-1020-18: geometry and grade, first choice for T-Max P and CoroTurn 107 (p. 2) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MM for ISO M, medium. Sandvik Coromant’s own catalog is the authority for its geometry.
It agrees with Sandvik Coromant’s catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)