Mitsubishi · uncoated carbide
UTi20T insert grade
UTi20T is Mitsubishi’s uncoated carbide grade (Uncoated) for ISO P25–P40, M25–M40 and K20–K35, as Mitsubishi’s catalog prints it. Uncoated carbide for steel, stainless and cast iron.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- uncoated carbide
- Coating
- Uncoated
- Substrate
- WC-TiC-TaC-Co, 90.5 HRA
- ISO P
- P25–P40 (core P35) · steel
- ISO M
- M25–M40 (core M35) · stainless steel
- ISO K
- K20–K35 (core K30) · cast iron
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
UTi20T equivalents by material
Steel · P
Read at P35, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1028 | PVD-coated carbide | PVD, TiAlN + TiN | P20–P50 | One source: ISCAR, its own catalog |
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why UTi20T for steel
UTi20T for steel: rated P25–P40 (core P35) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates UTi20T (uncoated carbide) for P25–P40 (core P35): Uncoated carbide for steel, stainless and cast iron.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
Stainless · M
Read at M35, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC228 | PVD-coated carbide | PVD, AlTiN + TiN | M30–M40 | One source: ISCAR, its own catalog |
| Kennametal | KCM35 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M30–M40 | One source: Kennametal, its own catalog |
| Sandvik | GC2035 | PVD-coated carbide | PVD | M25–M40 (core M35) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why UTi20T for austenitic stainless (304, 316)
UTi20T for austenitic stainless (304, 316): rated M25–M40 (core M35) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi rates UTi20T (uncoated carbide) for M25–M40 (core M35): Uncoated carbide for steel, stainless and cast iron.
One source: Mitsubishi Materials, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Cast iron · K
Read at K30, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | K20–K40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | K20–K30 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why UTi20T for gray cast iron
UTi20T for gray cast iron: rated K20–K35 (core K30) by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates UTi20T (uncoated carbide) for K20–K35 (core K30): Uncoated carbide for steel, stainless and cast iron.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists UTi20T at P20, P30, M20, M30, K20, K30. Mitsubishi Materials’ own catalog is the authority for its grade.
- The cross-reference lists P20; Mitsubishi Materials gives P25–P40.
- The cross-reference lists M20; Mitsubishi Materials gives M25–M40.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)