ISCAR · PVD-coated carbide

IC830 insert grade

IC830 is ISCAR’s PVD-coated carbide grade (PVD, AlTiN + TiN (SUMOTEC)) for ISO P20–P40, M25–M35 and S15–S30, as ISCAR’s catalog prints it. Interrupted and heavy cuts in steel, stainless and high-temperature alloys.

One source: ISCAR, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P, M and S.cutting edgecoating PVDsubstrate carbideISO groupPMS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
PVD-coated carbide
Coating
PVD, AlTiN + TiN (SUMOTEC)
ISO P
P20–P40 · steel
ISO M
M25–M35 · stainless steel
ISO S
S15–S30 · superalloys and titanium
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC830

IC830 equivalents by material

Steel · P

Read at P30, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P30
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNP20–P30

One source: Kennametal, its own catalog

MitsubishiVP15TFPVD-coated carbidePVDP20–P40 (core P30)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why IC830 for steel

IC830 for steel: rated P20–P40 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC830 (PVD-coated carbide) for P20–P40: Interrupted and heavy cuts in steel, stainless and high-temperature alloys.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. ISCAR — eCatalog grade data: IC830

Stainless · M

Read at M30, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M30
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNM20–M30

One source: Kennametal, its own catalog

MitsubishiVP15TFPVD-coated carbidePVDM20–M40 (core M30)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDM10–M30 (core M25)

One source: Sandvik Coromant, its own catalog

SecoCP600PVD-coated carbidePVD, (Ti,Al)N + TiNabout M20–M40

One source: Seco Tools, its own catalog

Why IC830 for austenitic stainless (304, 316)

IC830 for austenitic stainless (304, 316): rated M25–M35 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC830 (PVD-coated carbide) for M25–M35: Interrupted and heavy cuts in steel, stainless and high-temperature alloys.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC830

Superalloys · S

Read at S25, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S25
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNS20–S30

One source: Kennametal, its own catalog

MitsubishiMP9025PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS15–S35 (core S25)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDS20–S30 (core S25)

One source: Sandvik Coromant, its own catalog

Seco883micro-grain carbideUncoatedabout S10–S30

One source: Seco Tools, its own catalog

Why IC830 for heat-resistant superalloys (Inconel 718)

IC830 for heat-resistant superalloys (Inconel 718): rated S15–S30 by ISCAR.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC830 (PVD-coated carbide) for S15–S30: Interrupted and heavy cuts in steel, stainless and high-temperature alloys.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC830

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC830 at P20, P30, P40, M20, M30, K10, K20, K30, S20, S30. ISCAR’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)