Seco · PVD-coated carbide
TS2000 insert grade
TS2000 is Seco’s PVD-coated carbide grade (PVD, (Ti,Al)N + TiN) for ISO M01–M10 and S05–S20, as Seco’s catalog prints it. Finishing superalloys and titanium, and many stainless steels.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- PVD-coated carbide
- Coating
- PVD, (Ti,Al)N + TiN
- Substrate
- Hard micrograin
- ISO M
- about M01–M10 · stainless steel
- ISO S
- about S05–S20 · superalloys and titanium
- Secondary
- ISO P, K, H (Seco names them in its text only)
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
TS2000 equivalents by material
Stainless · M
Read at M05, the centre of Seco’s M range (stainless steel). Each grade is one its own maker rates for M05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC520 | PVD-coated carbide | PVD, TiCN + TiN | M05–M15 | One source: ISCAR, its own catalog |
| Mitsubishi | AP25N | cermet | PVD | M05–M25 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
Why TS2000 for austenitic stainless (304, 316)
TS2000 for austenitic stainless (304, 316): rated about M01–M10 by Seco.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Seco rates TS2000 (PVD-coated carbide) for about M01–M10: Finishing superalloys and titanium, and many stainless steels.
One source: Seco Tools, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
Superalloys · S
Read at S15, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1008 | PVD-coated carbide | PVD, AlTiN + TiN | S10–S20 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
Why TS2000 for heat-resistant superalloys (Inconel 718)
TS2000 for heat-resistant superalloys (Inconel 718): rated about S05–S20 by Seco.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Seco rates TS2000 (PVD-coated carbide) for about S05–S20: Finishing superalloys and titanium, and many stainless steels.
One source: Seco Tools, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists TS2000 at P10, M10, K10, K20, S10. Seco Tools’ own catalog is the authority for its grade.
It agrees with Seco Tools’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)