ISCAR · PVD-coated carbide
IC520 insert grade
IC520 is ISCAR’s PVD-coated carbide grade (PVD, TiCN + TiN) for ISO M05–M15, N05–N15 and S05–S20, as ISCAR’s catalog prints it. Austenitic stainless, high-temperature alloys and titanium.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, TiCN + TiN
- Substrate
- Hard
- ISO M
- M05–M15 · stainless steel
- ISO N
- N05–N15 · non-ferrous
- ISO S
- S05–S20 · superalloys and titanium
- Operations
- turning, milling
IC520 equivalents by material
Stainless · M
Read at M10, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M01–M10 | One source: Seco Tools, its own catalog |
Why IC520 for austenitic stainless (304, 316)
IC520 for austenitic stainless (304, 316): rated M05–M15 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC520 (PVD-coated carbide) for M05–M15: Austenitic stainless, high-temperature alloys and titanium.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC520
Non-ferrous · N
Read at N10, the centre of ISCAR’s N range (non-ferrous). Each grade is one its own maker rates for N10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5410 | PVD-coated carbide | PVD, TiB2 | N05–N20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why IC520 for aluminum
IC520 for aluminum: rated N05–N15 by ISCAR.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC520 (PVD-coated carbide) for N05–N15: Austenitic stainless, high-temperature alloys and titanium.
One source: ISCAR, the maker of the grade , sources [3]
Superalloys · S
Read at S15, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why IC520 for heat-resistant superalloys (Inconel 718)
IC520 for heat-resistant superalloys (Inconel 718): rated S05–S20 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC520 (PVD-coated carbide) for S05–S20: Austenitic stainless, high-temperature alloys and titanium.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC520
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC520 at M10. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)