ISCAR · PVD-coated carbide
IC228 insert grade
IC228 is ISCAR’s PVD-coated carbide grade (PVD, AlTiN + TiN) for ISO P25–P50, M30–M40, K20–K50, N20–N40 and S25–S30, as ISCAR’s catalog prints it. Steel and stainless at low to medium speed.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, AlTiN + TiN
- Substrate
- Very tough
- ISO P
- P25–P50 · steel
- ISO M
- M30–M40 · stainless steel
- ISO K
- K20–K50 · cast iron
- ISO N
- N20–N40 · non-ferrous
- ISO S
- S25–S30 · superalloys and titanium
- Operations
- turning, milling
IC228 equivalents by material
Steel · P
Read at P40, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P40 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | P20–P40 (core P30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why IC228 for steel
IC228 for steel: rated P25–P50 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC228 (PVD-coated carbide) for P25–P50: Steel and stainless at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
Stainless · M
Read at M35, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM35 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M30–M40 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2035 | PVD-coated carbide | PVD | M25–M40 (core M35) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why IC228 for austenitic stainless (304, 316)
IC228 for austenitic stainless (304, 316): rated M30–M40 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC228 (PVD-coated carbide) for M30–M40: Steel and stainless at low to medium speed.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC228
Cast iron · K
Read at K35, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | K20–K40 (core K30) | One source: Mitsubishi Materials, its own catalog |
Why IC228 for gray cast iron
IC228 for gray cast iron: rated K20–K50 by ISCAR.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC228 (PVD-coated carbide) for K20–K50: Steel and stainless at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
Non-ferrous · N
Read at N30, the centre of ISCAR’s N range (non-ferrous). Each grade is one its own maker rates for N30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | N20–N30 | One source: Kennametal, its own catalog |
Why IC228 for aluminum
IC228 for aluminum: rated N20–N40 by ISCAR.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC228 (PVD-coated carbide) for N20–N40: Steel and stainless at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
Superalloys · S
Read at S30, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | S20–S30 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9025 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S15–S35 (core S25) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | S20–S30 (core S25) | One source: Sandvik Coromant, its own catalog |
| Seco | 883 | micro-grain carbide | Uncoated | about S10–S30 | One source: Seco Tools, its own catalog |
Why IC228 for heat-resistant superalloys (Inconel 718)
IC228 for heat-resistant superalloys (Inconel 718): rated S25–S30 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC228 (PVD-coated carbide) for S25–S30: Steel and stainless at low to medium speed.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC228
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC228 at P30, P40, M30, K20, K30, S20. ISCAR’s own catalog is the authority for its grade.
- The cross-reference lists S20; ISCAR gives S25–S30.