ISCAR · PVD-coated carbide

IC250 insert grade

IC250 is ISCAR’s PVD-coated carbide grade (PVD, TiCN + TiN) for ISO P15–P35 and M20–M40, as ISCAR’s catalog prints it. High loads, medium to high speed.

One source: ISCAR, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P and M.cutting edgecoating PVDsubstrate carbideISO groupPM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
PVD-coated carbide
Coating
PVD, TiCN + TiN
ISO P
P15–P35 · steel
ISO M
M20–M40 · stainless steel
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC250

IC250 equivalents by material

Steel · P

Read at P25, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P25
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNP20–P30

One source: Kennametal, its own catalog

MitsubishiMS6015PVD-coated carbidePVDP10–P30 (core P20)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why IC250 for steel

IC250 for steel: rated P15–P35 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC250 (PVD-coated carbide) for P15–P35: High loads, medium to high speed.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. ISCAR — eCatalog grade data: IC250

Stainless · M

Read at M30, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M30
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNM20–M30

One source: Kennametal, its own catalog

MitsubishiVP15TFPVD-coated carbidePVDM20–M40 (core M30)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDM10–M30 (core M25)

One source: Sandvik Coromant, its own catalog

SecoCP600PVD-coated carbidePVD, (Ti,Al)N + TiNabout M20–M40

One source: Seco Tools, its own catalog

Why IC250 for austenitic stainless (304, 316)

IC250 for austenitic stainless (304, 316): rated M20–M40 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC250 (PVD-coated carbide) for M20–M40: High loads, medium to high speed.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC250

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC250 at P01, P10, P20, P30, M10, M30, M40. ISCAR’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)