Kennametal · CVD-coated carbide

KCP40 insert grade

KCP40 is Kennametal’s CVD-coated carbide grade (CVD, Thin MTCVD TiCN-Al2O3) for ISO P35–P45 and M20–M30, as Kennametal’s catalog prints it. Heavy roughing of carbon, alloy and stainless steel, including demanding interrupted cuts.

One source: Kennametal, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO P and M.cutting edgecoating CVDsubstrate carbideISO groupPM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Kennametal prints

Type
CVD-coated carbide
Coating
CVD, Thin MTCVD TiCN-Al2O3
Substrate
Tough carbide
ISO P
P35–P45 · steel
ISO M
M20–M30 · stainless steel
Operations
turning
Twin
KCP40B (CVD, Thin MTCVD TiCN-Al2O3-TiOCN): Kennametal prints the same range and use

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

KCP40 equivalents by material

Steel · P

Read at P40, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P40 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P40
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC635CVD-coated carbideCVD, TiN + TiC + TiNP30–P50

One source: ISCAR, its own catalog

MitsubishiUTi20Tuncoated carbideUncoatedP25–P40 (core P35)

One source: Mitsubishi Materials, its own catalog

SandvikGC4335CVD-coated carbideCVDP25–P45 (core P35)

One source: Sandvik Coromant, its own catalog

Why KCP40 for steel

KCP40 for steel: rated P35–P45 by Kennametal.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. So

    Kennametal rates KCP40 (CVD-coated carbide) for P35–P45: Heavy roughing of carbon, alloy and stainless steel, including demanding interrupted cuts.

    One source: Kennametal, the maker of the grade , sources [5]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  5. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Stainless · M

Read at M25, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC4050CVD-coated carbideCVD, TiCN + Al2O3 + TiNM20–M30

One source: ISCAR, its own catalog

MitsubishiMC7025CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM20–M40 (core M30)

One source: Mitsubishi Materials, its own catalog

SandvikGC2025CVD-coated carbideCVDM15–M35 (core M25)

One source: Sandvik Coromant, its own catalog

SecoTM2501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M20–M25

One source: Seco Tools, its own catalog

Why KCP40 for austenitic stainless (304, 316)

KCP40 for austenitic stainless (304, 316): rated M20–M30 by Kennametal.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal rates KCP40 (CVD-coated carbide) for M20–M30: Heavy roughing of carbon, alloy and stainless steel, including demanding interrupted cuts.

    One source: Kennametal, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists KCP40 at P40, M30. Kennametal’s own catalog is the authority for its grade.

It agrees with Kennametal’s catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)