ISCAR · PVD-coated carbide

IC908 insert grade

IC908 is ISCAR’s PVD-coated carbide grade (PVD, TiAlN) for ISO P15–P30, M20–M30, K20–K30, S10–S25 and H20–H30, as ISCAR’s catalog prints it. General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

One source: ISCAR, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P, M, K, S and H.cutting edgecoating PVDsubstrate carbideISO groupPMKSH
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
PVD-coated carbide
Coating
PVD, TiAlN
Substrate
Tough submicron
ISO P
P15–P30 · steel
ISO M
M20–M30 · stainless steel
ISO K
K20–K30 · cast iron
ISO S
S10–S25 · superalloys and titanium
ISO H
H20–H30 · hardened steel
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC908

IC908 equivalents by material

Steel · P

Read at P25, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P25
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNP20–P30

One source: Kennametal, its own catalog

MitsubishiMS6015PVD-coated carbidePVDP10–P30 (core P20)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why IC908 for steel

IC908 for steel: rated P15–P30 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC908 (PVD-coated carbide) for P15–P30: General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. ISCAR — eCatalog grade data: IC908

Stainless · M

Read at M25, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M25
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNM20–M30

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDM10–M30 (core M20)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDM10–M30 (core M25)

One source: Sandvik Coromant, its own catalog

SecoCP500PVD-coated carbidePVD, (Ti,Al)N + TiNabout M10–M30

One source: Seco Tools, its own catalog

Why IC908 for austenitic stainless (304, 316)

IC908 for austenitic stainless (304, 316): rated M20–M30 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC908 (PVD-coated carbide) for M20–M30: General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC908

Cast iron · K

Read at K25, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K25
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNK20–K30

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDK10–K30 (core K20)

One source: Mitsubishi Materials, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why IC908 for gray cast iron

IC908 for gray cast iron: rated K20–K30 by ISCAR.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC908 (PVD-coated carbide) for K20–K30: General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. ISCAR — eCatalog grade data: IC908

Superalloys · S

Read at S20, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S20
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNS10–S20

One source: Kennametal, its own catalog

MitsubishiMP9015PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS05–S25 (core S15)

One source: Mitsubishi Materials, its own catalog

SandvikGC1115PVD-coated carbidePVDS15–S25 (core S20)

One source: Sandvik Coromant, its own catalog

SecoCP200PVD-coated carbidePVD, (Ti,Al)N + TiNabout S10–S20

One source: Seco Tools, its own catalog

Why IC908 for heat-resistant superalloys (Inconel 718)

IC908 for heat-resistant superalloys (Inconel 718): rated S10–S25 by ISCAR.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC908 (PVD-coated carbide) for S10–S25: General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC908

Hardened · H

Read at H25, the centre of ISCAR’s H range (hardened steel). Each grade is one its own maker rates for H25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

No other maker’s verified grade covers H25 yet.

Why IC908 for hardened steel

IC908 for hardened steel: rated H20–H30 by ISCAR.

The reasoning, step by step
  1. The situation

    Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC908 (PVD-coated carbide) for H20–H30: General use on steel, austenitic stainless and high-temperature alloys over a wide speed range.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO H hardened steel
  2. Mitsubishi Materials — Machining course: ISO group H, hardened steel
  3. ISCAR — eCatalog grade data: IC908

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC908 at P10, P20, M20, K20, K30, S01, S10, S20, H20. ISCAR’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)