Kennametal · PVD-coated carbide
KCU25 insert grade
KCU25 is Kennametal’s PVD-coated carbide grade (PVD, AlTiN) for ISO P20–P30, M20–M30, K20–K30, N20–N30 and S20–S30, as Kennametal’s catalog prints it. General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, its own catalog
What Kennametal prints
- Type
- PVD-coated carbide
- Coating
- PVD, AlTiN
- Substrate
- Fine-grain unalloyed carbide
- ISO P
- P20–P30 · steel
- ISO M
- M20–M30 · stainless steel
- ISO K
- K20–K30 · cast iron
- ISO N
- N20–N30 · non-ferrous
- ISO S
- S20–S30 · superalloys and titanium
- Operations
- turning
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
KCU25 equivalents by material
Steel · P
Read at P25, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC250 | PVD-coated carbide | PVD, TiCN + TiN | P15–P35 | One source: ISCAR, its own catalog |
| Mitsubishi | MS6015 | PVD-coated carbide | PVD | P10–P30 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4325 | CVD-coated carbide | CVD | P10–P40 (core P25) | One source: Sandvik Coromant, its own catalog |
Why KCU25 for steel
KCU25 for steel: rated P20–P30 by Kennametal.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCU25 (PVD-coated carbide) for P20–P30: General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, the maker of the grade , sources [3]
Stainless · M
Read at M25, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC808 | PVD-coated carbide | PVD, TiAlN/AlTiN + TiN (SUMOTEC) | M20–M30 | One source: ISCAR, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | M10–M30 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M10–M30 | One source: Seco Tools, its own catalog |
Why KCU25 for austenitic stainless (304, 316)
KCU25 for austenitic stainless (304, 316): rated M20–M30 by Kennametal.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Kennametal rates KCU25 (PVD-coated carbide) for M20–M30: General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
Cast iron · K
Read at K25, the centre of Kennametal’s K range (cast iron). Each grade is one its own maker rates for K25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC808 | PVD-coated carbide | PVD, TiAlN/AlTiN + TiN (SUMOTEC) | K20–K30 | One source: ISCAR, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | K10–K30 (core K20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why KCU25 for gray cast iron
KCU25 for gray cast iron: rated K20–K30 by Kennametal.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCU25 (PVD-coated carbide) for K20–K30: General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, the maker of the grade , sources [3]
Non-ferrous · N
Read at N25, the centre of Kennametal’s N range (non-ferrous). Each grade is one its own maker rates for N25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC228 | PVD-coated carbide | PVD, AlTiN + TiN | N20–N40 | One source: ISCAR, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why KCU25 for aluminum
KCU25 for aluminum: rated N20–N30 by Kennametal.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCU25 (PVD-coated carbide) for N20–N30: General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, the maker of the grade , sources [3]
Superalloys · S
Read at S25, the centre of Kennametal’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC328 | PVD-coated carbide | PVD, TiCN | S20–S30 | One source: ISCAR, its own catalog |
| Mitsubishi | MP9025 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S15–S35 (core S25) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | S20–S30 (core S25) | One source: Sandvik Coromant, its own catalog |
| Seco | 883 | micro-grain carbide | Uncoated | about S10–S30 | One source: Seco Tools, its own catalog |
Why KCU25 for heat-resistant superalloys (Inconel 718)
KCU25 for heat-resistant superalloys (Inconel 718): rated S20–S30 by Kennametal.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Kennametal rates KCU25 (PVD-coated carbide) for S20–S30: General machining of steel, stainless, high-temperature alloys, titanium, iron and non-ferrous; interrupted cuts and high feeds.
One source: Kennametal, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists KCU25 at P30, M30, K20, K30, S20. Kennametal’s own catalog is the authority for its grade.
It agrees with Kennametal’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)