Kennametal · uncoated carbide

K68 insert grade

K68 is Kennametal’s uncoated carbide grade (Uncoated) for ISO M10–M20, K05–K20, N10–N20 and S10–S20, as Kennametal’s catalog prints it. Abrasion resistant: cast iron, austenitic stainless, non-ferrous; an alternative to K313 in high-temperature alloys.

One source: Kennametal, its own catalog

The cutting edge of a uncoated carbide insert in section: the carbide substrate, uncoated; rated for ISO M, K, N and S.cutting edgesubstrate carbideISO groupMKNS
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Type
uncoated carbide
Coating
Uncoated
Substrate
Hard, low-binder, alloyed WC/Co, fine grain
ISO M
M10–M20 · stainless steel
ISO K
K05–K20 · cast iron
ISO N
N10–N20 · non-ferrous
ISO S
S10–S20 · superalloys and titanium
Operations
turning

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

K68 equivalents by material

Stainless · M

Read at M15, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC07uncoated carbideUncoatedM10–M20

One source: ISCAR, its own catalog

MitsubishiAP25NcermetPVDM05–M25

One source: Mitsubishi Materials, its own catalog

SandvikGC1115PVD-coated carbidePVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

SecoTM1501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M10–M20

One source: Seco Tools, its own catalog

Why K68 for austenitic stainless (304, 316)

K68 for austenitic stainless (304, 316): rated M10–M20 by Kennametal.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal rates K68 (uncoated carbide) for M10–M20: Abrasion resistant: cast iron, austenitic stainless, non-ferrous; an alternative to K313 in high-temperature alloys.

    One source: Kennametal, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Cast iron · K

Read at K15, the centre of Kennametal’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedK10–K20

One source: ISCAR, its own catalog

MitsubishiHTi10uncoated carbideUncoatedK10–K20

One source: Mitsubishi Materials, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why K68 for gray cast iron

K68 for gray cast iron: rated K05–K20 by Kennametal.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal rates K68 (uncoated carbide) for K05–K20: Abrasion resistant: cast iron, austenitic stainless, non-ferrous; an alternative to K313 in high-temperature alloys.

    One source: Kennametal, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Non-ferrous · N

Read at N15, the centre of Kennametal’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for N15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC08uncoated carbideUncoatedN10–N20

One source: ISCAR, its own catalog

MitsubishiHTi10uncoated carbideUncoatedN10–N20

One source: Mitsubishi Materials, its own catalog

SandvikH10uncoated carbideUncoatedN01–N25 (core N15)

One source: Sandvik Coromant, its own catalog

Why K68 for aluminum

K68 for aluminum: rated N10–N20 by Kennametal.

The reasoning, step by step
  1. The situation

    Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    It wants a sharp edge with low cutting force, one chips don’t weld to.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  3. So

    Kennametal rates K68 (uncoated carbide) for N10–N20: Abrasion resistant: cast iron, austenitic stainless, non-ferrous; an alternative to K313 in high-temperature alloys.

    One source: Kennametal, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO N non-ferrous
  2. Mitsubishi Materials — Machining course: ISO group N, non-ferrous metals
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Superalloys · S

Read at S15, the centre of Kennametal’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedS05–S20

One source: ISCAR, its own catalog

MitsubishiMT9015uncoated carbideUncoatedS05–S25 (core S15)

One source: Mitsubishi Materials, its own catalog

SandvikH13Auncoated carbideUncoatedS10–S30 (core S15)

One source: Sandvik Coromant, its own catalog

SecoHXuncoated carbideUncoatedabout S10–S25

One source: Seco Tools, its own catalog

Why K68 for heat-resistant superalloys (Inconel 718)

K68 for heat-resistant superalloys (Inconel 718): rated S10–S20 by Kennametal.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal rates K68 (uncoated carbide) for S10–S20: Abrasion resistant: cast iron, austenitic stainless, non-ferrous; an alternative to K313 in high-temperature alloys.

    One source: Kennametal, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists K68 at M10, M20, K01, K10, K20, N10, N20, S10, S20. Kennametal’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)