Kennametal · PVD-coated carbide
KCS10 insert grade
KCS10 is Kennametal’s PVD-coated carbide grade (PVD, AlTiN) for ISO P10–P20, M10–M20, K05–K20, N10–N20, S10–S20 and H10–H10, as Kennametal’s catalog prints it. Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, its own catalog
What Kennametal prints
- Type
- PVD-coated carbide
- Coating
- PVD, AlTiN
- Substrate
- Fine-grained tungsten carbide
- ISO P
- P10–P20 · steel
- ISO M
- M10–M20 · stainless steel
- ISO K
- K05–K20 · cast iron
- ISO N
- N10–N20 · non-ferrous
- ISO S
- S10–S20 · superalloys and titanium
- ISO H
- H10–H10 · hardened steel
- Operations
- turning
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
KCS10 equivalents by material
Steel · P
Read at P15, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC903 | PVD-coated carbide | PVD, AlTiN | P10–P20 | One source: ISCAR, its own catalog |
| Mitsubishi | MS6015 | PVD-coated carbide | PVD | P10–P30 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why KCS10 for steel
KCS10 for steel: rated P10–P20 by Kennametal.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCS10 (PVD-coated carbide) for P10–P20: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [3]
Stainless · M
Read at M15, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | M05–M20 | One source: ISCAR, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M10–M30 | One source: Seco Tools, its own catalog |
Why KCS10 for austenitic stainless (304, 316)
KCS10 for austenitic stainless (304, 316): rated M10–M20 by Kennametal.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Kennametal rates KCS10 (PVD-coated carbide) for M10–M20: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
Cast iron · K
Read at K15, the centre of Kennametal’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC903 | PVD-coated carbide | PVD, AlTiN | K10–K20 | One source: ISCAR, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | K10–K30 (core K20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why KCS10 for gray cast iron
KCS10 for gray cast iron: rated K05–K20 by Kennametal.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCS10 (PVD-coated carbide) for K05–K20: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [3]
Non-ferrous · N
Read at N15, the centre of Kennametal’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC907 | PVD-coated carbide | PVD, TiAlN | N05–N20 | One source: ISCAR, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why KCS10 for aluminum
KCS10 for aluminum: rated N10–N20 by Kennametal.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCS10 (PVD-coated carbide) for N10–N20: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [3]
Superalloys · S
Read at S15, the centre of Kennametal’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1008 | PVD-coated carbide | PVD, AlTiN + TiN | S10–S20 | One source: ISCAR, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why KCS10 for heat-resistant superalloys (Inconel 718)
KCS10 for heat-resistant superalloys (Inconel 718): rated S10–S20 by Kennametal.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Kennametal rates KCS10 (PVD-coated carbide) for S10–S20: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
Hardened · H
Read at H10, the centre of Kennametal’s H range (hardened steel). Each grade is one its own maker rates for H10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | H05–H15 | One source: ISCAR, its own catalog |
| Seco | TH1000 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | about H05–H15 | One source: Seco Tools, its own catalog |
Why KCS10 for hardened steel
KCS10 for hardened steel: rated H10–H10 by Kennametal.
The reasoning, step by step
The situation
Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KCS10 (PVD-coated carbide) for H10–H10: Engineered for high-temperature alloys, at speeds about double those of conventional PVD grades.
One source: Kennametal, the maker of the grade , sources [3]