Mitsubishi · cermet
NX2525 insert grade
NX2525 is Mitsubishi’s cermet grade (Uncoated) for ISO P10–P25, M10–M25 and K10–K25, as Mitsubishi’s catalog prints it. Cermet for steel, stainless and ductile iron finishing; for dry cutting.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- cermet
- Coating
- Uncoated
- Substrate
- 92.2 HRA
- ISO P
- P10–P25 (core P15) · steel
- ISO M
- M10–M25 (core M15) · stainless steel
- ISO K
- K10–K25 (core K15) · cast iron
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names NX2525 its first choice for carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), stable conditions: finishing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerNX2525 equivalents by material
Steel · P
Read at P15, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC30N | cermet | Uncoated | P10–P30 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | P10–P20 | One source: Kennametal, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why NX2525 for steel
NX2525 for steel: rated P10–P25 (core P15) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates NX2525 (cermet) for P10–P25 (core P15): Cermet for steel, stainless and ductile iron finishing; for dry cutting.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
Stainless · M
Read at M15, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC30N | cermet | Uncoated | M10–M20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | M10–M20 | One source: Kennametal, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M10–M20 | One source: Seco Tools, its own catalog |
Why NX2525 for austenitic stainless (304, 316)
NX2525 for austenitic stainless (304, 316): rated M10–M25 (core M15) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi rates NX2525 (cermet) for M10–M25 (core M15): Cermet for steel, stainless and ductile iron finishing; for dry cutting.
One source: Mitsubishi Materials, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Cast iron · K
Read at K15, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC20 | uncoated carbide | Uncoated | K10–K20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | K05–K20 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why NX2525 for gray cast iron
NX2525 for gray cast iron: rated K10–K25 (core K15) by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates NX2525 (cermet) for K10–K25 (core K15): Cermet for steel, stainless and ductile iron finishing; for dry cutting.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists NX2525 at P10, P20, M10, M20, K01, K10, K20. Mitsubishi Materials’ own catalog is the authority for its grade.
- The cross-reference lists K01; Mitsubishi Materials gives K10–K25.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)