Mitsubishi · PVD-coated carbide
VP20RT insert grade
VP20RT is Mitsubishi’s PVD-coated carbide grade (PVD) for ISO M20–M40, K20–K40 and S15–S35, as Mitsubishi’s catalog prints it. Tough PVD grade; stainless, cast iron and heat resistant alloys in interrupted cuts.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- PVD-coated carbide
- Coating
- PVD
- ISO M
- M20–M40 (core M30) · stainless steel
- ISO K
- K20–K40 (core K30) · cast iron
- ISO S
- S15–S35 (core S25) · superalloys and titanium
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
VP20RT equivalents by material
Stainless · M
Read at M30, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1028 | PVD-coated carbide | PVD, TiAlN + TiN | M20–M40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | M20–M30 | One source: Kennametal, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | M10–M30 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why VP20RT for austenitic stainless (304, 316)
VP20RT for austenitic stainless (304, 316): rated M20–M40 (core M30) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Mitsubishi rates VP20RT (PVD-coated carbide) for M20–M40 (core M30): Tough PVD grade; stainless, cast iron and heat resistant alloys in interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Cast iron · K
Read at K30, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | K20–K40 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | K20–K30 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why VP20RT for gray cast iron
VP20RT for gray cast iron: rated K20–K40 (core K30) by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates VP20RT (PVD-coated carbide) for K20–K40 (core K30): Tough PVD grade; stainless, cast iron and heat resistant alloys in interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
Superalloys · S
Read at S25, the centre of Mitsubishi’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC328 | PVD-coated carbide | PVD, TiCN | S20–S30 | One source: ISCAR, its own catalog |
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | S20–S30 | One source: Kennametal, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | S20–S30 (core S25) | One source: Sandvik Coromant, its own catalog |
| Seco | 883 | micro-grain carbide | Uncoated | about S10–S30 | One source: Seco Tools, its own catalog |
Why VP20RT for heat-resistant superalloys (Inconel 718)
VP20RT for heat-resistant superalloys (Inconel 718): rated S15–S35 (core S25) by Mitsubishi.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Mitsubishi rates VP20RT (PVD-coated carbide) for S15–S35 (core S25): Tough PVD grade; stainless, cast iron and heat resistant alloys in interrupted cuts.
One source: Mitsubishi Materials, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists VP20RT at P20, P30, M20, M30, K20, K30, S30. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)